title: What is the Difference between Narrowband and Wideband Irradiance Control?
description: "In Xenon and UV fluorescent accelerated weathering testing, an irradiance setpoint value is incomplete information without reference to the wavelength or wavelength range it represents. There are two classes of irradiance setpoints: Narrowband and Wideband. Read more to find out the differences between each."
image: https://blog.q-lab.com/hubfs/graph_narrowband_wideband_2.jpg
---

[![q-lab-loog-standlards-landing](https://blog.q-lab.com/hs-fs/hubfs/Logos%20and%20Assets/q-lab-loog-standlards-landing.png?width=150&name=q-lab-loog-standlards-landing.png "q-lab-loog-standlards-landing")](https://blog.q-lab.com/)

- [Q-Lab.com](https://www.q-lab.com)
- [Testing Services](https://q-lab.com/test-services/)
- [Products](https://q-lab.com/products/)

# Q-Lab Weathering & Corrosion Blog

Read the latest news and articles from the experts.

#### Filter Posts by Category

- [Weathering](https://blog.q-lab.com/tag/weathering)
- [Corrosion](https://blog.q-lab.com/tag/corrosion)
- [FAQ](https://blog.q-lab.com/tag/faq)
- [Outdoor](https://blog.q-lab.com/tag/outdoor)
- [Case Study](https://blog.q-lab.com/tag/case-study)

# What is the Difference between Narrowband and Wideband Irradiance Control?

Posted by [Bill Tobin](https://blog.q-lab.com/author/bill-tobin) on Jun 19, 2020 10:37:32 AM

In Xenon and UV fluorescent accelerated weathering testing, an irradiance setpoint value is incomplete information without reference to the wavelength or wavelength range it represents. There are two classes of irradiance setpoints.

**Narrowband **irradiance setpoints include 340 nm and 420 nm, and represent a 1 nm wide bandpass, centered on the single wavelength value indicated (i.e. ½ nm on either side of 340 nm, for example). Narrowband irradiances use units of “Watts per square meter per nanometer.” This can be written as either W/(m2∙nm), W/m2/nm, or W∙m-2∙nm-1.

**Wideband **irradiance setpoints (usually “TUV” or “total UV”) are an integration of the irradiance from all wavelengths between two endpoints, usually 300-400 nm (accelerated laboratory) or 295-385 nm (outdoor). As a result, wideband irradiance values are generally much larger than narrowband irradiance values. Wideband irradiance is measured in “Watts per square meter,” written as W/m2 or W∙m-2.

The graph below is a **spectral power distribution** (SPD), which presents irradiance as a function of wavelength. This SPD shows that, for this particular light source, one could describe the irradiance either as having a narrowband irradiance of 0.35 W/m2/nm @ 340 nm, OR as a wideband irradiance of 40 W/m2 from 300-400 nm (TUV).

![SPD Graph](https://q-lab.com/_cms-content/pagecontent/Images/narrow-widebandgraph-qtip11.PNG)

 Topics: [Weathering](https://blog.q-lab.com/topic/weathering?hsLang=en), [FAQ](https://blog.q-lab.com/topic/faq?hsLang=en)

- [Tweet](https://twitter.com/share)

**Q-Lab Corporation is a global provider of material durability testing products. We design and manufacture Q-PANEL standard test substrates as well as weathering, light stability, and corrosion testers. Q-Lab also offers A2LA accredited contract test services, including accelerated laboratory testing. Our weathering products and services are used by materials scientists, research and development engineering, and quality control personnel in numerous industries.**

[Read More](https://q-lab.com/about/)

- [Q-Lab.com](https://www.q-lab.com)
- [QUV Accelerated Weathering Test Chambers](https://q-lab.com/products/quv-weathering-tester/quv)
- [Q-SUN Xenon Test Chambers](https://q-lab.com/products/q-sun-xenon-arc-test-chambers)
- [Q-FOG Corrosion test Chambers](https://q-lab.com/products/q-fog-cyclic-corrosion-chamber)
- [Testing Services](https://q-lab.com/test-services/)

Subscribe To Notification Updates

### Subscribe to update notifications

<https://www.facebook.com/qlabweathering/> <https://twitter.com/qlabweathering> <https://www.linkedin.com/company/q-lab-corporation>

© 2026 Q-Lab Corporation

![Tagline_CMYKBlue_Logo_Left](https://blog.q-lab.com/hs-fs/hubfs/Logos%20and%20Assets/Tagline_CMYKBlue_Logo_Left.png?width=300&name=Tagline_CMYKBlue_Logo_Left.png "Tagline_CMYKBlue_Logo_Left")